{"_buckets": {"deposit": "c7946838-3a2b-4952-89b5-96dec21af940"}, "_deposit": {"created_by": 3, "id": "2009", "owners": [3], "pid": {"revision_id": 0, "type": "depid", "value": "2009"}, "status": "published"}, "_oai": {"id": "oai:shinshu.repo.nii.ac.jp:00002009", "sets": []}, "author_link": ["6024", "6027", "6023", "6021", "6028", "6022", "6025", "6029", "6031", "6026", "6030", "6020"], "item_20002_alternative_title_1": {"attribute_name": "その他(別言語等)のタイトル", "attribute_value_mlt": [{"subitem_alternative_title": "Mechanical Properties and Metal Dissolution of Laser-Welded Titanium in Physiological Saline and Lactic Acid"}]}, "item_20002_biblio_info_27": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "1995-08-30", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "2", "bibliographicPageEnd": "147", "bibliographicPageStart": "137", "bibliographicVolumeNumber": "21", "bibliographic_titles": [{"bibliographic_title": "松本歯学"}]}]}, "item_20002_creator_2": {"attribute_name": "作成者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "山岸, 利夫"}], "nameIdentifiers": [{"nameIdentifier": "6020", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "竹内, 勝泉"}], "nameIdentifiers": [{"nameIdentifier": "6021", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "森, 厚二"}], "nameIdentifiers": [{"nameIdentifier": "6022", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "横山, 宏太"}], "nameIdentifiers": [{"nameIdentifier": "6023", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "伊藤, 充雄"}], "nameIdentifiers": [{"nameIdentifier": "6024", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "孔, 泰寛"}], "nameIdentifiers": [{"nameIdentifier": "6025", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "津村, 智信"}], "nameIdentifiers": [{"nameIdentifier": "6026", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "丹羽, 健"}], "nameIdentifiers": [{"nameIdentifier": "6027", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "出口, 敏雄"}], "nameIdentifiers": [{"nameIdentifier": "6028", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "林, 春二"}], "nameIdentifiers": [{"nameIdentifier": "6029", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "五十嵐, 順正"}], "nameIdentifiers": [{"nameIdentifier": "6030", "nameIdentifierScheme": "WEKO"}]}]}, "item_20002_date_19": {"attribute_name": "日付", "attribute_value_mlt": [{"subitem_date_issued_datetime": "2012-05-24", "subitem_date_issued_type": "Created"}]}, "item_20002_description_14": {"attribute_name": "内容記述", "attribute_value_mlt": [{"subitem_description": "This study investigated tensile and releasing properties of titanium samples which were laser welded, plasma welded, and infra-red soldered after immersing test. The main results obtained are as follows; The insertion of a titanium foil was effective to prevent volume reduction during the welding process. It was found that the laser welding reduces tensile properties, especially toughness, and elongation when the samples were immersed and shaken in a physiological saline and in a lactic acid prior to the laser welding. It was also found that, even self-welded titanium samples would be embrittled when they were placed in a corrosive environment over a long period of time. The magnitude of these reductions was more significant with the silver soldering than those with titanium soldering. No evidence of titanium released from the welded portion was observed in a physiological saline, but the released amount of titanium from the welded portion was higher than that from the base metal when it was exposed to a lactic solution. After a silver soldering, a trace amount of titanium was released in a physiological saline after a 6-month immersion test, and the lactic acid\u0027s released titanium was remarkably greater with the laser-welded samples. In addition to titanium, it was observed that copper and zinc released from the soldering material were detected in larger amounts.", "subitem_description_type": "Other"}]}, "item_20002_description_21": {"attribute_name": "フォーマット", "attribute_value_mlt": [{"subitem_description": "application/pdf", "subitem_description_type": "Other"}]}, "item_20002_full_name_16": {"attribute_name": "公開者(その他言語)", "attribute_value_mlt": [{"nameIdentifiers": [{"nameIdentifier": "6031", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "松本歯科大学学会"}]}]}, "item_20002_identifier_23": {"attribute_name": "資源識別子URI", "attribute_value_mlt": [{"subitem_identifier_type": "URI", "subitem_identifier_uri": "http://id.nii.ac.jp/1070/00000864/"}]}, "item_20002_source_id_25": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "0385-1613", "subitem_source_identifier_type": "ISSN"}]}, "item_20002_source_id_26": {"attribute_name": "処理レコードID(総合目録DB)", "attribute_value_mlt": [{"subitem_source_identifier": "AN00232590", "subitem_source_identifier_type": "NCID"}]}, "item_20002_text_52": {"attribute_name": "機関ID", "attribute_value_mlt": [{"subitem_text_value": "6"}]}, "item_20002_text_53": {"attribute_name": "コンテンツID", "attribute_value_mlt": [{"subitem_text_value": "oai:mdu.repo.nii.ac.jp:00000864"}]}, "item_20002_text_54": {"attribute_name": "コンテンツ更新日時", "attribute_value_mlt": [{"subitem_text_value": "2022-09-07T00:56:52Z"}]}, "item_20002_version_type_51": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_970fb48d4fbd8a85", "subitem_version_type": "VoR"}]}, "item_access_right": {"attribute_name": "アクセス権", "attribute_value_mlt": [{"subitem_access_right": "metadata only access", "subitem_access_right_uri": "http://purl.org/coar/access_right/c_14cb"}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"download_preview_message": "", "file_order": 0, "filename": "", "future_date_message": "", "is_thumbnail": false, "mimetype": "", "size": 0, "url": {"url": "https://mdu.repo.nii.ac.jp/?action=repository_action_common_download\u0026item_id=864\u0026item_no=1\u0026attribute_id=22\u0026file_no=1"}, "version_id": ""}]}, "item_keyword": {"attribute_name": "キーワード", "attribute_value_mlt": [{"subitem_subject": "チタン", "subitem_subject_scheme": "Other"}, {"subitem_subject": "レーザ溶接", "subitem_subject_scheme": "Other"}, {"subitem_subject": "赤外線ろう付", "subitem_subject_scheme": "Other"}, {"subitem_subject": "プラズマ溶接", "subitem_subject_scheme": "Other"}, {"subitem_subject": "浸漬試験", "subitem_subject_scheme": "Other"}, {"subitem_subject": "溶出", "subitem_subject_scheme": "Other"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "journal article", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "レーザ溶接したチタンの浸漬溶液中における機械的性質の経時的変化と溶出について", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "レーザ溶接したチタンの浸漬溶液中における機械的性質の経時的変化と溶出について"}]}, "item_type_id": "20002", "owner": "3", "path": ["2400"], "permalink_uri": "https://shinshu.repo.nii.ac.jp/records/2009", "pubdate": {"attribute_name": "公開日", "attribute_value": "2022-11-10"}, "publish_date": "2022-11-10", "publish_status": "0", "recid": "2009", "relation": {}, "relation_version_is_last": true, "title": ["レーザ溶接したチタンの浸漬溶液中における機械的性質の経時的変化と溶出について"], "weko_shared_id": -1}
レーザ溶接したチタンの浸漬溶液中における機械的性質の経時的変化と溶出について
https://shinshu.repo.nii.ac.jp/records/2009
https://shinshu.repo.nii.ac.jp/records/200955a5089b-6025-4b0a-bd35-3b4b7a31be08
名前 / ファイル | ライセンス | アクション |
---|---|---|
https://mdu.repo.nii.ac.jp/?action=repository_action_common_download&item_id=864&item_no=1&attribute_id=22&file_no=1
|
|
Item type | Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2022-11-10 | |||||
タイトル | ||||||
タイトル | レーザ溶接したチタンの浸漬溶液中における機械的性質の経時的変化と溶出について | |||||
その他(別言語等)のタイトル | ||||||
その他のタイトル | Mechanical Properties and Metal Dissolution of Laser-Welded Titanium in Physiological Saline and Lactic Acid | |||||
作成者 |
山岸, 利夫
× 山岸, 利夫× 竹内, 勝泉× 森, 厚二× 横山, 宏太× 伊藤, 充雄× 孔, 泰寛× 津村, 智信× 丹羽, 健× 出口, 敏雄× 林, 春二× 五十嵐, 順正 |
|||||
公開者(その他言語) | ||||||
姓名 | 松本歯科大学学会 | |||||
書誌情報 |
松本歯学 巻 21, 号 2, p. 137-147, 発行日 1995-08-30 |
|||||
言語 | ||||||
言語 | jpn | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | チタン | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | レーザ溶接 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | 赤外線ろう付 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | プラズマ溶接 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | 浸漬試験 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | 溶出 | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||
資源タイプ | journal article | |||||
アクセス権 | ||||||
アクセス権 | metadata only access | |||||
アクセス権URI | http://purl.org/coar/access_right/c_14cb | |||||
内容記述 | ||||||
内容記述タイプ | Other | |||||
内容記述 | This study investigated tensile and releasing properties of titanium samples which were laser welded, plasma welded, and infra-red soldered after immersing test. The main results obtained are as follows; The insertion of a titanium foil was effective to prevent volume reduction during the welding process. It was found that the laser welding reduces tensile properties, especially toughness, and elongation when the samples were immersed and shaken in a physiological saline and in a lactic acid prior to the laser welding. It was also found that, even self-welded titanium samples would be embrittled when they were placed in a corrosive environment over a long period of time. The magnitude of these reductions was more significant with the silver soldering than those with titanium soldering. No evidence of titanium released from the welded portion was observed in a physiological saline, but the released amount of titanium from the welded portion was higher than that from the base metal when it was exposed to a lactic solution. After a silver soldering, a trace amount of titanium was released in a physiological saline after a 6-month immersion test, and the lactic acid's released titanium was remarkably greater with the laser-welded samples. In addition to titanium, it was observed that copper and zinc released from the soldering material were detected in larger amounts. | |||||
日付 | ||||||
日付 | 2012-05-24 | |||||
日付タイプ | Created | |||||
フォーマット | ||||||
内容記述タイプ | Other | |||||
内容記述 | application/pdf | |||||
資源識別子URI | ||||||
識別子 | http://id.nii.ac.jp/1070/00000864/ | |||||
識別子タイプ | URI | |||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 0385-1613 | |||||
処理レコードID(総合目録DB) | ||||||
収録物識別子タイプ | NCID | |||||
収録物識別子 | AN00232590 | |||||
著者版フラグ | ||||||
出版タイプ | VoR | |||||
出版タイプResource | http://purl.org/coar/version/c_970fb48d4fbd8a85 |